It was flat when I put it on the mold, my purpose was to prevent devit as it was slumping; I took it up to a higher temperature than usual in a slump to get a better fire polish (I realize I was taking a shortcut- and I see that’s not a good idea!)

Thanks for the feedback, I appreciate your thoughts.