It depends upon the shape
Home › Forums › FusedGlass.Org Website Help › Forum Help › Bent corner › It depends upon the shape
December 26, 2016 at 3:58 am #13674
Participant
It depends upon the shape and the mold you are slumping into, but most likely, it will not flatten. Either refuse flat, or cold work the edge to remove the bend (which means you may need to cold work all edges).
Dana W.
Fused Glass Designs
dba Jester’s Baubles