It allows air to escape and
Home › Forums › Glass Fusing › General Fusing Discussion › New eBook! › It allows air to escape and
April 18, 2013 at 4:34 pm #12876
Inactive
It allows air to escape and guarantees no bubbles between the shelf and glass.