Is your intial heating very

Home Forums Glass Fusing General Fusing Discussion Top Layer is Sliding! Is your intial heating very

#12775
Anonymous
Inactive

Is your intial heating very fast (full speed)?

If so, I’d be curious if slowing down fixes the problem. ¬†Rapid expansion (of the glass, of the shelf, etc.) is (relatively) rapid movement.

The thin glass is probably a contributing factor: lighter glass = easier to move.



Paul