If you use it, only use a very small amount. I ruined a whole batch of pendants once. They all had discolored spots on them. It took me a moment to figure out why and then it dawned on me. Every dot of glue left a discolored spot right in the middle of the piece. I don’t use glue at all now. I can see with the textured dichro a little tiny dab would help. I think you can even dilute the glue a bit. Hope that helps.