If you kiln shelf is smooth,
Home › Forums › Glass Fusing › General Fusing Discussion › Back side of glass › If you kiln shelf is smooth,
October 15, 2010 at 6:33 pm #11736
Participant
If you kiln shelf is smooth, you can use thinfire ( a Bullseye product), if you have the coarser paper, you can smooth it by adding kiln wash to it and smoothing it level. If you are working small, you can grind and polish the back to get it smooth, too.
Stephen Richard
blogs at: http://www.verrier-glass.blogspot.com/ and http://www.glasstips.blogspot.com/