If you have some polishing

#12152
petra kaiser
Participant

If you have some polishing bits on your grinder or some diamond hand polishing sponges you could pre-polish them a little bit and than they will fire polish at an even  lower temperature. Around 1300 F.

petra kaiser – http://www.kaiserlee.com –¬†