I would lengthen the hold
Home › Forums › Glass Fusing › General Fusing Discussion › Fold-over pendants › I would lengthen the hold
December 27, 2013 at 9:46 pm #13148
Inactive
I would lengthen the hold time. The best thing to do is peek every so often until they have bent sufficiently.