I use E6000 the same way
Home › Forums › Glass Fusing › General Fusing Discussion › Glue for fused glass jewelry › I use E6000 the same way
September 5, 2008 at 2:56 pm #10614
Participant
I use E6000 the same way Petra does for earrings, roughing up all surfaces the glue will be applied to, then letting it cure without touching or moving for 48 hours & rarely have the finding come off. For pendants I’m now drilling & using pinch bails to avoid glue altogether.