I use any two part epoxy
Home › Forums › Glass Fusing › General Fusing Discussion › HELP! Need a great glue for metal to glass › I use any two part epoxy
September 6, 2008 at 3:51 am #10712
Participant
I use any two part epoxy that dries clear. Rough up both glass and metal where it is to be glued. Be sure you mix equal parts and stir until it is no longer clear. Apply quickly. I put the item under the heat lamp to cure. Check before it gets too hard if you need to reposition. I use this on all jewelry, wine stoppers,letter openers. etc.The best part, you can buy this at any hardware store for less than $5.00. Bev