I never slump over 1150 —

Home Forums Glass Fusing General Fusing Discussion slumping large disks I never slump over 1150 —

#10515
TerryC
Participant

I never slump over 1150 — the temperature plus time will soften and slump the glass.  I’d
rather have to have a longer hold than risk it by going to hot.

Good luck
Terry Curtis