I have the MK wet saw with
Home › Forums › Glass Fusing › General Fusing Discussion › wet saw problem › I have the MK wet saw with
I have the MK wet saw with the best blade for glass but still had the problem At a class with Bullseye they had the same saw but they put a plastic top to the table. So I thought ‘bounce’ with just putting the glass directly on the table was the cause & expermented with various table tops. Everything from foam board (Pretty good but gets soggy) so bought this white rigid pvc sheet half inch thick & it works best but the slot in your table material needs to be cut with the saw so its an exact fit. You also need to fix it to the sliding table pretty good. Yes a sacrificial piece of glass under works good too but you sure waste a lot of glass.