I have done a flip and fire

Home Forums Glass Fusing General Fusing Discussion I have a bubble – sad face. I have done a flip and fire

#13091
Vernelle
Participant

I have done a flip and fire and gotten rid of smaller bubbles.   Doesn’t always work but worth a try.

 

I flip and fire


if the bubbles go away ..I fire again on the design side to get the glossy look.