I have also had one bad “run” of glass, that devited every time I fired it. I have a couple of other glasses that tend to cloud a little, and I usually make sure that I cap them rather than have them as the top surface. Of the two that I cap, one is a Uroborus dark purple, and another is a Spectrum 96 white that strikes to beige.