I have a olympic 146gfe
Home › Forums › Glass Fusing › General Fusing Discussion › Glass fracturing › I have a olympic 146gfe
May 28, 2011 at 11:55 am #12078
Participant
I have a olympic 146gfe 120v. This has happened during drapes to form a vase and slumps in several different plate molds and also flat tack fuse of two sheets of glass. Usually the bottom plate when tack fusing breaks. I assume the bottom plate just is not heating due to the top plate acting as an insulator. Thanks for any help!
Keith