I had a similar problem with

Home Forums Glass Fusing General Fusing Discussion Kiln Wash Application Problem I had a similar problem with

#12198
glassbymargot
Participant

I had a similar problem with a shelf once. I fired the shelf in my kiln to1500 degrees F. Whatever was on the shelf preventing it from taking on the kiln wash burned off. Not sure if this will help but but may be worth a try.