I fully fuse usually at 1480 (Bullseye say 1490) & I found the old MR-97 was OK with transparent but had a bloom just like a mild devit on opals. I believe its only ‘good’ for 1440 which means a long hold to fully fuse & thats not good. You want to spend the shortest time at full process temp.