I believe if you polled most fused glass artists (without their lawyers present) they would tell you they fire at night while the sleep and even when they go out of the house briefly.
Make sure to follow all the safety precautions (there is a good review on this site here).
For years I fired my kiln at night with the controller alarm set to 25 degrees above the highest temp in the program and a baby monitor by the kiln and on my night stand. The idea is that if you ever have a “runaway” kiln, the alarm will go off and you’ll hear it.