http://www.youtube.com/watch?v=VXR1M-X_akU please try this link. You can get Aloe in any place where they sell sun lotion – it is good against sun burn. You mix it one part powder, one part aloe and some clean water to thin it down. You can also buy fritz Spritz or Liquid Stringer Medium from your glass supplier.