Hi,
thank you for using Kaiser Lee Board. If you have any of my books you also have instructions on how to use it. Please send me an email and I will email you some instructions in pdf format. petra@kaiserlee.com. The only problem with other kiln wash products is that they are sticking to glass once in a while and than the KLB will stick to the kiln wash. If you never have problems with kiln wash sticking to your glass, than you can use it with your KL board as well. Have a happy New Year
petra