It is pretty much impossible to fuse glass with zero respiratory risks. The good news is that the risk is very manageable.
All fiber products (including shelf paper) and shelf primer produce ariborne particules that are unhealthy to breath. I consider a high quality respirator (rated N99 or N100) and a HEPA vacuum filter mandatory studio equipment.