Hi DeDa.
Been fusing for multiple years using BE kilnwash, and reuse the wash for multiple firings. I found that if you drop tmperature about 20 degrees with a full fuse, increase soak time to compensate for the temp difference, you won’t have sticking. Could also be sticking due to type of glass, I’ve found opals have kiln wash stick more that other types.