Here is the link to
Home › Forums › Glass Fusing › General Fusing Discussion › fusing schedule for 1-1/2″ x 1-1/2″ x 16″ pattern bar › Here is the link to
January 5, 2012 at 3:07 am #12369
Participant
Here is the link to Bullseye’s annealing recommendation/schedule:
http://www.bullseyeglass.com/images/stories/bullseye/PDF/TechNotes/technotes_07.pdf
I would use this to modify the schedule you have for the 1″ thick piece. Go slower on the ramp up and hold longer at process temp and during the anneal, then go down more slowly.
Of course, if you are using another manufacturer’s glass, you should check to see if they have similar charts.