grey goose
Home › Forums › Glass Fusing › General Fusing Discussion › sluming grey goose bottles › grey goose
June 28, 2015 at 10:42 pm #13513
Participant
just my way of doing it–i sandblast most of the printing from the back of the bottle–also put a piece of thinfire under the printing so it does not stick to the shelf–then you must scrape and recoat the shelf–tou know how tha goes–good luck
Pete