graphite in the kiln
Home › Forums › Glass Fusing › General Fusing Discussion › Graphite in the kiln? › graphite in the kiln
September 27, 2010 at 5:03 pm #11722
Participant
I got some fun shapes of graphite off eBay, and I did try them in the kiln. I took a very interesting piece out of the kiln, but the smell was INTENSE. I wouldn’t do it again with the kiln in the house, but *maybe* in a VERY WELL VENTILATED area.
Although the pieces of graphite I used were somewhat “fragile”, they lasted though a firing (pot melt temp) quite nicely.