I have been using gold leaf in some of my kilnformed work for a while now. I sandwich it between two layers of glass with success as well as letting it fuse into the top layer. I use small pieces (about the size of a finger nail or less) and sometimes sprinkle some colored frit on top. it works nicely…try it!