Have you tried to roughen both sides a bit and than clean them with alcohol befor you apply the glue? E 6000 seems to be the glue so far – but it is not a 100% guaranty this is the reason, why I favor glass pendants without any glue on bails. (but it seems I’m old fashioned minority in this field when you see all the bails on the market.
have fun
petra kaiser