Glass used in stained glass
Home › Forums › Glass Fusing › General Fusing Discussion › Newbie having trouble › Glass used in stained glass
August 27, 2014 at 4:51 am #13413
Participant
Glass used in stained glass can be all different brands, Spectrum, Kokomo, Wissmach, etc. They will not mix. They will shatter when combined. You need to try glass from the same piece together. They may turn an ugly color but maybe you could still find out the temperature ranges on the kiln