Temps for kiln carving are hotter than slumping and tack fusing. Bullseye has a tip sheet on kiln carving:
http://www.bullseyeglass.com/methods-ideas/tipsheet-1-kilncarving.html
Dana
Jester’s Baubles Fused Glass Designs