Glass glue
Home › Forums › Glass Fusing › General Fusing Discussion › Glue for fused glass jewelry › Glass glue
September 5, 2008 at 3:08 pm #10616
Participant
I came to glass via the Lapidary route. I used to make Opal triplets and Doublets. The glue I used was Epoxy 330. It holds very well, especially if the surfaces are not polished. It can be heated to accelerate the curing time, and most importantly, it cures "waterclear." I have used it on glass with great success. It would work perfectly for the bales.