glass edges
Home › Forums › Glass Fusing › General Fusing Discussion › Clearing up the Edges › glass edges
November 4, 2012 at 8:21 am #12148
Participant
I have diamond hand pads that I bought through Delphi that come in 4 different grits and work nicely for cleaning up the edges after grinding. scrubbing the edges is still essential and keep the sponge that wets your grinder clean. That helps too.