July 18, 2012 at 4:12 am #12537
Participant
I fused 4 one inch penants and all four stuck to the mold. I had kiln-washed the mold before using. Looking online many mentioned heating the mold/glass up in the kiln to 1000 while having the mold upside down. I found an alternative and much quicker solution that worked for me. I put the mold in the freezer for 15-20 minutes. When I pulled the mold out and flipped it over all four pieces dropped out when tapped. Plan B would have been to reheat! Julie