Fusing w/Argentium silver
Home › Forums › Glass Fusing › General Fusing Discussion › argentium › Fusing w/Argentium silver
February 19, 2011 at 8:08 pm #11941
Participant
Hi, I wrap pendants w/Argentium silver, 21 gauge square, so tried it in fusing (to make bails held between the top and bottom piece)….NO, it doesn’t work!!! It just turns black and melty. Stick with sterling silver, fine silver, stainless or copper for it to work…