August 23, 2010 at 1:02 am #11697
Participant
Hi Paul,
The glass popped off in some areas. While the actual suncatcher remained in tack. It was the dichroic detail that popped off around 1089 degrees.
I took a peek through one of my peep wholes and noticed that a few of the dichroic pieces had popped off and flipped over. The pieces I’m speaking of are very, very small. When I realized what had happened I aborted my firing.
After the kiln cooled I repositioned the pieces and fired again with no problems. I was just wondering what might have caused this to happen.
Denise