 No…you do not have to fire polish the pieces.  That will happen as you fire.  You might also want to take a look at the suggested firing schedules that Paul has in the “Tools” section above and go from there.

I would definitely listen to Stephen’s advice…both about tack fusing and the possibility that this project may not be a great success. 

 

 

 

 