fusing objects in glass
Home › Forums › Glass Fusing › General Fusing Discussion › Fusing objects into the glass. › fusing objects in glass
June 19, 2013 at 1:24 pm #12762
Participant
Try lowering your fusing temp about 20deg F and lengthening your time some. I have been doing this for a while now with most everything and am much happier with the results.