June 30, 2011 at 1:25 am #12128
Participant
I have a new small jewelry casting mold, a teardrop shape with a raised area for a hole. (My first experiment with frit) I filled it with frit and when finished, it had “burrs” all around the edges from the frit. I fired slowly to 1600 degrees and then left it until cool. Did I not fire it hot enough or what? I’m new at this.
Thank you,
Jan