Fusing glass bottles
Home › Forums › Glass Fusing › General Fusing Discussion › Fusing glass bottles › Fusing glass bottles
August 25, 2012 at 3:18 am #12655
Participant
Others have highly recommended this book. I haven’t read it (not really into glass bottles):
http://www.amazon.com/Best-Bottle-Book-Ever-Boyce/dp/0982584725
Other than that, it’s all about experimentation and keeping good records of your firing schedules and results. If they are not as rounded as you would like, try hotter or longer (or both).
Dana W.
Jester’s Baubles Fused Glass Designs