I go to the dollar store and get the White Rain, pump not aresol, hair spray. Pour a little in a cup and use a tooth pick to put a drop on the bottom edge of the frit as it is setting on your base piece. You will see the liquid seep under the glass. Let dry about 10-15 mintues.
Vernelle