Hi There:
I found your post very helpful. I just did my first fusing with the fusible transfer paper that I bought from Delphi. Everything looks great, with the exception that I can slightly see the outline of where the edge of the paper meets the glass. I fired (3) 2 3/4″ X 1 1/2′ pieces in my small Evenheat kiln to 1350 F. I held it there for about 5 minutes before I turned it off. This fusbile paper came with instructions, except for any actual fusing instructions with temperatures or time. I did some investigating online & around 1350 F seemed to be what I could find & that firing much higher might burn off the photo fusing image. If I still see the outline – does that mean I should fire it longer? Hotter?
Thanks for any additional help!