Fossil Vitra

#11557
Tosca
Participant

 June Askew

It looks lovely, I want to look at this lesson.  A few years ago I did an experiment with maiden hair fern (native Australian plant grows near creeks).  I decided to put it between two sheets of float glass.  I applied one piece, then the remaining one was accidently soaked in alcohol (for cleaning

purposes only).  After being fired I was happy to see that one piece was black, the other one was pure white so it looked very good.  I hope some give it a try with some American plants, it will

be something new I expect.

Tosca