For the most common shapes and projects, a 100F/hour climb to 1200F with no hold will give decent results.  We use this in our teaching studios across a huge variety of projects with consistent success.

That being said, those advocating to make your decision by observing the glass are absolutely correct that that is the way you get the best results.