Follow up
Home › Forums › Glass Fusing › General Fusing Discussion › Kiln wash stuck to glass › Follow up
May 13, 2017 at 1:48 pm #13704
Participant
I found some suggestions to try. CLR prompted no change. Etching cream while sanding, and then refiring, did!I was able to resolve my problem and save the piece.