float glass firing schedules

Home Forums FusedGlass.Org Website Help Forum Help Float glass firing schedules float glass firing schedules

#12522
kazelis
Participant

Many thanks for your advice.  Fusing schedule very similar to the one I use (My top temp. for 2layers of 3mm glass is 827 degrees, but annealing is the same) I was wondering about the slumping schedule.  Will try it out and let you know.

Regards,

Glass-The workshop