Flat front to channel
Home › Forums › Glass Fusing › General Fusing Discussion › How do I make a channel for something in the back so the front is flat › Flat front to channel
January 16, 2013 at 9:30 pm #12802
Participant
You can get a flat front on your channel by putting the whole project on 3mm fibre paper with a slot cut out where the rod will be (the fibre paper during firing). This will allow the glass to fall into the gap leaving the front flat. There are other ways of course.
Stephen Richard
blogs at: http://www.verrier-glass.blogspot.com/ and http://www.glasstips.blogspot.com/