oh well, I waited for the temperature to rise to1224F then used my dental tool to put a small hole in the bubble. It relaxed. There is a slight ripple in it now so, will have to think on it. May just incorporate it into the design. Will see. Doesn’t look the way I wanted it to hwr, it may just turn out to be a happy accident.