Firing schedules vary from kiln to kiln. For some good information, check out Bullseye’s tech notes. I’d recommend you start with Heat and Glass (http://www.bullseyeglass.com/images/stories/bullseye/PDF/TechNotes/TechNote_4_2012.pdf) or knowing your kiln ( http://www.bullseyeglass.com/images/stories/bullseye/PDF/TechNotes/technotes_01.pdf)
Terry Curtis