Thanks for your help Dana. 2012-10-21
Ramp Goal temp. hold
R1 300 degrees 1150 degrees 30min.
R2 500 1475 15min.
R3 9999 1150 10 min.
R4 500 960 30min.
For Slumping a soap dish, I tried the following twice!
R1 400 1000 20min.
R2 400 1250 60min.
R3 9999 950 60min.
R4 400 100 0min.