Hi Paul,

I am a fairly new fuser and have just joined this forum – so bear with me if I don’t get it right on my first try…(in fact, I believe I originally posted this question in the wrong place. So technically, this is my 2nd try!)  )  Your fossil vitra tutorial got my attention immediately and I can’t wait to try it. 

 Quick question on the firing schedule:  The hold column shows 60 min at 900F but the text refers to a half hour hold.  Is a 30 min hold normally sufficient to burn off plant material, hairspray, etc?  Thanks so much.