August 10, 2013 at 10:21 pm #13034
Participant
I would fire hotter for a shorter time – maybe 50°F for 20′. I would also go afap to the anneal soak.
However, there is a high possibility of devitrification on second and subsequent firings of float.
Stephen Richard
blogs at: http://www.verrier-glass.blogspot.com/ and http://www.glasstips.blogspot.com/